What is it about?

This work investigates the effect of heat treatment on the joint toughness of 302 austenitic stainless steel. Therefore, this work determines the reason for the crack in the spot weld of stainless steel 302. The effect of heat treatment on different weld joints that have been welded at different currents. Therefore, the tensile shear strength is improved by annealing at temperatures up to 750 °C. However, at 850 °C, the tensile shear strength drops.

Featured Image

Why is it important?

The investigation of weld area properties of stainless steel and its strength

Perspectives

Little works dealing with austenitic stainless steel and the cracking in weld nugget

Dr. Ahmed Almukhtar

Read the Original

This page is a summary of: Effect of Heat Treatments on 302 Austenitic Stainless Steel Spot Weld, Advanced Engineering Forum, August 2018, Trans Tech Publications,
DOI: 10.4028/www.scientific.net/aef.29.19.