The addition of polylactic acid (PLA) pellets containig 15% carbon fibre (CF) into a SMP polyurethane increased the shape recovery flexural strees of the blend compared with the unreinforced polymer. The % of CF in blend is a trade off mechanical and shape memory properties. This lays the foundation to scale up 4D printing shape-shifting materials for engineering applications.

Featured Image

Read the Original

This page is a summary of: Direct 4D printing: pellet extrusion of shape memory polymer composites with large-scale additive manufacturing machine, Rapid Prototyping Journal, January 2026, Emerald,
DOI: 10.1108/rpj-07-2025-0313.