What is it about?

It is possible to use citric acid for removal of lead from flash smelting slag. Optimal conditions: 1 mol/dm3 of citric acid, 30 minutes, 70oC, l/s = 5.

Featured Image

Why is it important?

There are several advantages of the hydrometallurgical technology, namely the prospect of lower production costs, lower energy consumption and a higher recovery rate of lead from slag compared to conventional methods.

Read the Original

This page is a summary of: Leaching of lead and copper from flash smelting slag by citric acid, Archives of Civil and Mechanical Engineering, May 2019, Elsevier,
DOI: 10.1016/j.acme.2019.02.001.