What is it about?

The initial crack length (a i) was assumed to be equal to 0.1 mm in case of weld toe. This length was satisfactory for different butt joints geometries.

Featured Image

Why is it important?

Determine the initial crack length that influence on fatigue life. Also, Benchmarking result has been presented.

Perspectives

The simulation using Franc2d presented the validate results regarding the crack Propagation.

Dr. Ahmed Almukhtar

Read the Original

This page is a summary of: The Effect of Weld Profile and Geometries of Butt Weld Joints on Fatigue Life Under Cyclic Tensile Loading, Journal of Materials Engineering and Performance, October 2010, Springer Science + Business Media,
DOI: 10.1007/s11665-010-9775-1.
You can read the full text:

Read

Contributors

The following have contributed to this page