What is it about?
Despite its paramount importance in dictating long-term performance and safety of lithium-ion batteries (LIBs), the solid electrolyte interphase (SEI) on graphitic electrodes remains the least understood area in LIBs due to its dynamic nature, the complexity of chemical composition, heterogeneity in morphology, and the lack of reliable in situ/operando techniques for accurate characterization. SEI is formed due to electrolyte reduction and decomposition at the electrode surface during the initial cycles. The chemical composition and morphology of SEI are not only affected by the choice of electrolyte, but also by the nature of the electrode surface. While the introduction of defects (i.e., imperfections) into graphitic electrodes has been shown to improve their electrochemical properties, how such structural defects influence SEI formation and evolution remains an open question. In this work, we utilized non-destructive electrochemical Atomic Force Microscopy (EChem-AFM) to systematically monitor and compare the dynamic SEI formation and evolution on a pair of representative graphitic materials with and without defects, namely pseudo graphite from University of Idaho thermolyzed asphalt reaction (GUITAR) and highly oriented pyrolytic graphite (HOPG), respectively. Complementary to the characterization of topographical and mechanical changes of SEI during electrochemical cycling by EChem-AFM, ex situ chemical analysis by X-ray photoelectron spectroscopy (XPS) and density functional theory calculations were conducted to provide mechanistic insights underlying SEI formation and evolution. A comprehensive and dynamic picture of the formation and evolution of SEI on graphitic electrodes with and without defects is described. The SEI forms at the graphite with defects more readily compared to a perfect graphite electrode. The density functional theory (DFT) calculations suggest that the adsorption energy barrier of the ethylene carbonate solvent molecule bonded Li compound is much lower on a graphite surface with common point defects (e.g., Stone-Wales and single vacancy), leading to a lower decomposition energy barrier and thus a more positive onset potential. The defects in the graphite structure induce formation of a thinner, denser, and more uniform SEI, which also exhibits a stronger passivating ability and a good stability upon cycling. The SEI formed on the graphite with defects was rich in LiF, which has been reported as an effective passivating component in SEI on Li and Si electrode materials. In summary, our mechanistic study provides fundamental understandings as well as critical new insights into the SEI formation and evolution on graphite electrode materials with and without defects, which offers a new design strategy of engineered SEI for high performance LIB and beyond.
Featured Image
Why is it important?
Our current work provides new insights into the role of defects in graphitic electrodes for LIBs. Our fundamental study reveals the factors that promote a more passivating and stable SEI for graphitic electrodes for enhanced cycling stability.
Perspectives
Our work suggests that by modulating the point defects in graphitic electrode materials, one will be able to regulate the SEI composition, nucleation, and formation. A thinner, more robust and passivating SEI layer can be formed through enrichment of LiF for improved longevity of lithium-ion batteries. Thus, the graphite with defects can be designed as coatings onto other high-capacity electrodes such as Li, Si, and Sn, for a stable SEI. Furthermore, the graphite with the defects can be coated onto the conventional graphite electrodes to improve its rate performance and cycling stability for applications such fast charging batteries. Our study provides a fundamental understanding of SEI formation and evolution on graphite electrode materials with and without defects, which offers a new design strategy of engineered SEI for high performance LIB and beyond.
Claire Xiong
Boise State University
Read the Original
This page is a summary of: A Comparison of Solid Electrolyte Interphase Formation and Evolution on Highly Oriented Pyrolytic and Disordered Graphite Negative Electrodes in Lithium‐Ion Batteries, Small, October 2021, Wiley,
DOI: 10.1002/smll.202105292.
You can read the full text:
Contributors
The following have contributed to this page